Failure Analysis of a Pipe due to Internal Pressure
A three inch, Schedu1e 40 by 33 inches long, fresh water galvanized steel pipe, from the Astoria fuel depot, was submitted for a cause of failure analysis. The pipe was reported to have been in service for up to sixty years but a heat trace on the pipe…